Waiting on registration approval? Email me! daved223(at)yahoo.com
I think you can do it by electrolysis with the brass being the positive and a piece of copper the negative. Kind of a reverse plating.
Frank
Thanks Frank !
I am wondering what the appropriate plating solution would be ?
Sodium hydroxide (lye) and distilled water makes a base solution.
I think you can do it by electrolysis with the brass being the positive and a piece of copper the negative. Kind of a reverse plating. Frank
I checked my notes, the workpiece should be the negative, the opposite of what I previously posted.
Sorry Jerry, I use this process for rust removal and have a sticky note to remind me which is positive and what is negative because I never can remember!
i